A mining line is specified by duty, not by product name: what the solids are, how fast they have to move, and where the line has to be opened for maintenance. This page works through that order, then gives the families and the size tables that answer it.

dn20–dn1600butt fusion range
dn1400electrofusion coupler
Ø32–Ø355ball valves
SDR 11/17wall series

Why a mining line moves to PE, and where it does not

A slurry or tailings line is judged on two things a water main is not: how fast it wears out, and how quickly it can be put back into service. Every metre carries solids, and every shutdown stops the plant behind it. PE answers both, but not for the reason most catalogues give.

The first reason is corrosion. A steel slurry line fails from the inside out, and a PE line does not corrode at all, so the wall thickness you specify at year zero is the wall thickness at year twenty. The second is joint count. A PE line is delivered in 12 m lengths or coils and joined end to end, so a 4 km tailings line has a fraction of the joints a flanged steel line needs, and every joint that does not exist is a leak that cannot happen. The third is handling. PE weighs roughly one eighth of steel for the same bore, so the same excavator places a longer length, and a floating dredge line does not need the buoyancy a steel line would.

What PE does not do is resist coarse angular rock at any velocity. Wear in a slurry line scales with velocity to a power well above one, and with particle sharpness. Where the solids are crushed rock above a few millimetres and the line runs fast, the industry lines the bends with rubber or ceramic and keeps the PE for the straight runs, or accepts a scheduled bend replacement. The honest statement is that PE wins on fine and medium particle slurry at controlled velocity, on tailings, on return water, and on every line where corrosion is the failure mode rather than abrasion. Read the rest of this page that way: the fittings are chosen for the duty, not for the material name.

The tell is in the bends. If a line's maintenance record is full of bend replacements, the problem is velocity and geometry, not the pipe. Moving a 90° to two 45° at the same radius, or widening the bore at the bend, buys more life than upgrading the material grade.

The range, grouped by what the line asks of it

The families below are moulded in our own tooling. They are grouped by the job they do in a mining circuit rather than by product name, because that is how a line is actually specified: the main is butt fusion, the tie-ins are electrofusion, the branches are saddles, and the plant connections are flanged.

The mining package, grouped by the job each group does
Family groupFamiliesSize rangeSize entriesWhat it covers
Large-diameter butt fusion8dn20–dn1600350Elbows, tees, reducers, end caps, flange adaptors. The main haul, tailings and return lines.
Electrofusion, for tie-ins and repairs8dn20–dn1400264Couplings, elbows, tees and end caps that fuse without a machine in the trench.
Saddles, for a branch on a live line8dn63–dn40084Outlet, clamp and bypass saddles, dn63 to dn400 on the main.
Ball valves, for isolation3Ø32–Ø35527Standard port, single vent and double vent bodies with fusion ends.
Steel-to-PE transitions2dn25–dn35553The pump house and equipment connections, plain steel end, SDR11 and SDR17.
Stub ends and flange rings3dn40–dn160072Flanged joints where the PE side carries the ring or the stub.

Where each fitting sits in the circuit

A mining package is not one product. It is six or seven positions along a line, and each position fails for its own reason. This is the map we quote against.

Position in the circuit, fitting used, and why that fitting
PositionFitting that goes thereWhy this one
Pump discharge, first 20 mSteel-to-PE transition, then a butt fusion 90° or 45°Pressure pulsation is highest here, and the pump flange is steel. The transition is the only place the two materials meet.
Main haul or tailings runButt fusion pipe, elbows and tees, dn160 to dn1600Long straight runs with few joints. Butt fusion gives a joint with the same wall as the pipe, at the lowest cost per joint.
Branch to a second line or a sumpEqual or reducing tee, or an electrofusion saddleA tee if the line is being built; a saddle if the branch is added to a line that already carries slurry.
Tie-in to an existing lineElectrofusion coupling, dn20 to dn1400Electrofusion needs less clearance than a butt fusion machine, so it works in a trench that is already backfilled on one side.
Isolation before a plantPE ball valve, Ø32 to Ø355Fusion ends, so the valve is part of the line rather than a flanged break in it.
Plant, thickener or cyclone manifoldFlange adaptor with steel ring, or a stub end to a floating flangeThe plant side is always flanged and always steel. The question is whether the PE side carries the ring or the stub.
Floating dredge lineFlange adaptor at each pontoon joint, 45° elbows betweenA floating line moves. Flanged joints let a section be swapped without cutting the line.
Line end or future extensionButt fusion end capCloses the line for a hydrostatic test, and comes off when the next stage is built.

Velocity is the wear control, not the wall thickness

Two numbers set the life of a slurry line: the velocity that keeps the solids moving, and the velocity above which the bends start to pay for it. Below the first, solids settle and the line sands up. Above the second, wear at every direction change rises faster than the flow does. The window between them depends on particle size and on the solids concentration, so treat the table as a starting point for the hydraulic design, not as a specification.

Design velocity window by solids, as a starting point for the hydraulic model
Solids in the lineKeep aboveKeep belowWhat happens outside the window
Fine tailings, slimes, below about 0.1 mm1.0–1.5 m/s2.5–3.0 m/sBelow: the line sands up at the low points. Above: little extra wear, but the pump pays for a head that buys nothing.
Sand and silt, 0.1–0.5 mm1.5–2.0 m/s3.0–3.5 m/sThis is the band where PE performs best: the solids stay in suspension and the wall sees sliding rather than impact.
Fine gravel, 0.5–2 mm2.0–2.5 m/s3.5–4.0 m/sBends begin to show a wear pattern. Two 45° instead of one 90° at the same radius is the cheapest fix.
Coarse gravel and crushed rock, above 2 mm2.5–3.0 m/s4.0 m/s and upImpact wear dominates. Line the bends, or plan to replace them; the straight PE run is still the right choice.

Two practical notes that come out of this. A line that is oversized for its flow sits below the settling velocity and blocks; a line that is undersized wears and wastes head. And a bend is not a passive part: at the same velocity, a 90° elbow sees several times the wear of a 45°, because the particle stream hits it square on instead of glancing off. Where a line turns 90° on a plan drawing, two 45° elbows and a short spool usually outlast one 90° for a small extra material cost.

Choosing the bend: 90°, two 45°, or a wider radius

Three ways to turn a slurry line, and what each costs
OptionWear at the bendHead lossWhere it is the right answer
Single 90° elbowHighestHighestClean water, return lines, and any turn that can be taken out of the slurry path.
Two 45° elbows with a short spoolRoughly halvedLowerThe default for a slurry main. Two more joints, much longer bend life.
Fabricated wide-radius bendLowestLowestPermanent installations where a bend can be made off site and the plant cannot stop for a replacement.

Both 45° and 90° elbows are moulded up to dn900 in the electrofusion range and dn1600 in butt fusion, so the geometry is available without a special order. What is not available off the shelf is a wide-radius fabricated bend; that is a drawing, not a catalogue item.

How far the large-diameter range actually goes

Most suppliers of PE fittings stop at dn630 because that is where the injection moulds and the butt fusion machines stop being commodity items. The table below is what we mould, family by family, so a line can be specified at the size the hydraulic model asks for rather than the size the catalogue happens to carry.

Butt fusion families, size range and largest moulded entry
FamilySize rangeSizesLargest entryWhere it earns its place in a mining line
Butt Fusion Reducerdn50–dn63078dn630Reducing the main where the pump curve allows a smaller bore
Butt Fusion 90° Elbowdn20–dn160031dn1600Direction changes on the main haul line
Butt Fusion 45° Elbowdn50–dn160027dn1600Wear-free direction changes where a 90° would scour
Butt Fusion Equal Teedn40–dn160027dn1600Equal branch on a delivery main
Butt Fusion Reducing Teedn50–dn1600102dn1600Branch into a smaller line without a second reducer
Butt Fusion End Capdn20–dn160031dn1600Line end, future extension, hydrostatic test closure
Butt Fusion Flange Adapterdn40–dn160028dn1600Bolting to a pump, a valve or a plant manifold
Butt Fusion Flange Steel Ringdn40–dn120026dn1200The steel ring that backs the flange adaptor

Joining on site: which method, in which situation

A mining site usually needs three methods at once, because it is building new line, tying into old line, and repairing line that failed last week. The method is decided by access, not by preference.

Method by situation
SituationMethodWhat decides it
New main, open trench, dn63 and aboveButt fusionLowest cost per joint and a joint with the full pipe wall. Needs room for the machine on both sides of the joint.
Tie-in to a line already in serviceElectrofusion coupling or saddleNo facing tool and no machine travel, so it fits a bell hole. The fitting carries its own fusion parameters on the nameplate.
Repair after a puncture or a burstElectrofusion coupling, or a spool piece with two couplingsA coupling needs only the damaged section cut out and two clean ends. It is the fastest route back to pumping.
Instrument and wash-down lines, dn20 to dn63Socket fusionA hand-held heating tool instead of a machine, which is what a plant maintenance team already has.
Connection to a steel flangeFlange adaptor, or stub end with a backing ringDepends on whether the PE side is fixed or needs to be rotated during assembly.

What a mining package has to state before we can quote it

A mining enquiry that arrives as a pipe diameter and a length cannot be quoted accurately, because the fittings are the variable part. These are the lines that change the price, in the order they change it.

Ordering checklist
What to stateWhy it moves the price
Duty: tailings, slurry, return water, or dredgeSets the velocity window, and therefore the bore and the wall series.
Solids: particle size and concentrationDecides whether the bends are standard mouldings or a scheduled wear item.
Design pressure and test pressureFixes the SDR. A tailings line at 6 bar and a pump discharge at 16 bar are not the same fitting.
Diameter schedule, with the split at each branchReducing tees and reducers are quoted by combination, and the combination is the price.
Number and angle of every bendBends are the wear item and the largest single line in a mining fitting package.
Flange standard and drillingThe plant side is already built. A flange adaptor drilled to the wrong pattern is scrap.
Delivery sequenceA line is built from the pump outwards. Shipping the whole package at once usually means storing half of it on site.

Frequently asked questions

Is HDPE suitable for tailings lines?

Yes, and it is the common choice for fine and medium tailings. The material does not corrode, the joints are fusion joints rather than flanged, and a tailings line is usually low pressure, which is where PE is cheapest per metre. What has to be engineered is the velocity: too low and the line sands up, too high and the bends wear. The bore is chosen from the settling velocity of the solids, not from the pump size.

Will HDPE outlast steel in abrasive slurry?

In fine particle slurry, usually yes, because steel loses wall to corrosion as well as abrasion and PE only loses wall to abrasion. In coarse angular rock at high velocity, no: impact wear removes PE faster than it removes a hardened steel wall, which is why those lines use rubber or ceramic lined bends. The realistic answer is that PE wins the straight runs and the fine solids, and the bends are a wear item in either material.

What velocity should a slurry line run at?

Above the settling velocity of the solids and below the velocity where bend wear accelerates. For fine tailings that is roughly 1.0 to 2.5 m/s; for sand and silt about 1.5 to 3.5 m/s; for fine gravel 2.0 to 4.0 m/s. These are starting points for the hydraulic model, not a standard, and the particle size distribution is what decides the actual number.

Which fitting do I use at a pump connection?

A steel-to-PE transition fitting, because the pump flange is steel and the line is PE. The transition is a PE stub fusion-welded to a steel end, supplied with the steel length and the flange drilling you specify. On the discharge side it is worth adding a 45° rather than a 90° immediately after the transition, because that is where pulsation and the first wear both land.

Do you mould dn1600 fittings?

Yes, in butt fusion: equal tees, reducing tees, 90° and 45° elbows, end caps and flange adaptors are moulded up to dn1600, and the electrofusion coupling range goes to dn1400. The size is not the constraint; the machine that fuses it on site is, so a dn1600 package is usually quoted together with the fusion equipment and the operator training.

Can the line run above ground?

It can, with two changes. The pipe needs carbon black for UV resistance, and the pressure rating has to be derated for the service temperature, because PE loses strength as it warms and a black pipe in the sun runs hotter than the ambient air. Above-ground line also needs support at closer centres than buried line, because PE creeps under its own weight when warm.